TR 104

HI-TEMP MOLD RELEASE

An industry standard premium paste release for use in higher exothermic applications. Formulated using only the
highest quality refined carnauba wax, blended with other high temperature synthetic waxes and additives producing
the highest quality mold release wax for the composites market.

WHAT ARE YOU LOOKING FOR?
*
This field is required
Total quantity you need
*
This field is required
*
This field is required
Email format error
Due to email instability, you might miss our correspondence. Please provide your phone number for alternative contact.
This field is required
Telephone information is wrong!
Send Message
img of mask_layer_close
TR-104
Product Detail

PRODUCT Description:

TR-104 is TR Industries' industry-standard premium paste release for higher-exothermic molding applications. It is formulated using only the highest quality refined carnauba wax, blended with other high-temperature synthetic waxes and additives, positioning it as the higher-heat counterpart to TR Industries' standard-duty TR-102 Regular Mold ReleaseTR-104 is rated for use up to 215°F (102°C), versus 200°F (93°C) for TR-102, and dries to a harder film accordingly.

PRODUCT FEATURES:

★ Ease of application and removal – may be allowed to stand before polishing

★ Provides hard film with superior heat and chemical properties

★ Polishes to high gloss without streaking

★ Reduced wax build-up and styrene accumulation

PHYSICAL PROPERTIES:

Dry Time: 5-10 minutes@ 72°F. Varies depending on working temperature

Wax Melting or Softening Point: 195 - 210°F (88 - 99°C)

Penetration Hardness: 1 at 25°C (carnauba wax)

Color: light blue tint (color coded for identification)

VOC Content: 4.84lbs./gal (580g/l)

USES:

As a release agent for composite molding on all FRP tooling, metal and other hard surface molds.

★ Open mold hand or spray lay up

★ Resin Transfer/injection (RTM) & (RIM)

★ Vacuum bag and compression molding

★ Polyester & epoxy resins

Applications

On new or reconditioned tooling, TR recommends applying sealer glaze TR-301 or TR-910 semi-permanent sealer before waxing, for added release, gloss, and mold life. Apply the wax with a sponge applicator in a thin, even circular motion across the mold surface, allow to haze dry (approx. 5–10 minutes depending on ambient temperature), then polish to a gloss finish with a soft cloth (not microfiber). For new or reconditioned molds, apply a minimum of 6 coats of paste wax, waiting approximately 30–60 minutes between coats for the wax to set and harden after polishing.

Best results come from letting the mold stand overnight after waxing and applying a final coat the following day before gel coating, then applying a further coat of wax for the first 2–3 parts released. The number of parts producible before re-waxing is needed will vary with molding conditions, part configuration, resin, mold cycles, gel coat cure, and other factors.

Contact our Additives Team.jpg



    Cooperating Suppliers

    We cooperate with multiple well-known domestic suppliers

    Evergreen Chemicals Collaborating Brands.jpg


    Certificate Display

    Our products have passed various industry certifications

    Evergreenchemicals Qualification Certificate




    Inquire Now
    Name: *
    Mobile:
    E-mail: *
    Message: *
    Verification code: *
      

    Recommended Products

    ONE STOP SUPPLIER OF COMPOSITE MATERIALS
    Company Name
    *
    This field is required
    Email
    *
    This field is required
    Email format error
    Phone
    This field is required
    Telephone information is wrong!
    Message
    *
    This field is required
    Send Message